904L SS Plate is a high purity, low sulphur grade, and as such will not machine well. Despite this the grade can be machined using standard techniques.In most environments 904L SS Plate has a corrosion performance intermediate between the standard austenitic grade 316L and the very highly alloyed 6% molybdenum and similar "super austenitic" grades.In aggressive nitric acid 904L SS Plate has less resistance than molybdenum-free grades such as 304L and 310L.
Type No:904L SS Plate/Plates/Sheet/Sheets+904L SS Plates/Sheets+SS 904L Plates/Sheets+904L Steel Sheets/Plates
&&&Heat Treatment
&&&Welding
Type No:904L SS Plate/Plates/Sheet/Sheets+904L SS Plates/Sheets+SS 904L Plates/Sheets+904L Steel Sheets/Plates
1 | commodity | 904L SS Plate [Stainless Steel 904L Sheet/Plates] |
2 | material | 201, 202, 301,304, 304L, 316, 316L, 309S, 310,310S, 317L, 321, 409, 409L, 410, 420, 430,904,904L etc |
3 | surface | 2B, BA, HL, 4K, 6K, 8K, NO. 1, NO. 2, NO. 3, NO. 4, NO. 5,Pickling,Mirror |
4 | standard | AISI, ASTM, DIN, EN, GB, JIS, etc |
5 | advantage | (1) High surface quality, clean, smooth finish (2) Good corrosion resistance, durability than ordinary steel (3) High strength and to deform (4) Not easy to be oxidized (5) Good welding performance (6) The use of diversity |
6 | package | (1) Products are packed and labeled according to regulation (2) According to customers' requirement |
7 | delivery | within 7-15 days since we get the deposit, mainly according to your quantity and the ways of transportation |
8 | payment | T/T, L/C |
9 | shipment | FOB/CIF/CFR |
10 | productivity | 500tons/month |
11 | note | We can supply other grade products as customers' requirement. |
&&&Heat Resistance
Good resistance to oxidation, but like other highly alloyed grades suffers from structural instability (precipitation of brittle phases such as sigma) at elevated temperatures. 904L should not be used above about 400°C.
&&&Heat Treatment
Solution Treatment (Annealing) - heat to 1090-1175°C and cool rapidly. This grade cannot be hardened by thermal treatment.
&&&Welding
904L can be successfully welded by all standard methods. Care needs to be taken as this grade solidifies fully austenitic, so is susceptible to hot cracking, particularly in constrained weldments. No pre-heat should be used and in most cases post weld heat treatment is also not required. AS 1554.6 pre-qualifies Grade 904L rods and electrodes for welding of 904L.