Grade | C max | Si max | Mn | P max | S max | Als min | Ti max | Cu max | Cr max | Ni max | Mo max | Nb | V |
EH36 | 0.18 | 0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 | 0.02-0.05 | 0.05-0.10 |
Note: Generally speaking CE will be ≤0.40%. If the delivery condition is TMPC, the CE will be : ≤ 0.38% (thickness ≤ 50mm),≤0.40%( when the thickness >50-100). Ceq% =(C+Mn)/6+(Cr+Mo+V)/5+(Ni+Cu)/15.
Grade | Rm (MPa) | Re(MPa)min | A%min | Akv/Jmin | ||||||
EH36 | 490-630 | 355 | 21 | E.T°C | Thickness(mm) | |||||
-40 | ≤ 50 | >50-70 | >70-100 | |||||||
L | C | L | C | L | C | |||||
34 | 24 | 41 | 27 | 50 | 34 |
Note: In the list , Rm: .tensile strength,Re: Yield strength,A%: elongation, E.T: experimental temperature,L: lengthways, C: crosswise.
Grade | Fine grains elements | category | The thickness of steel | ||||||
≤ 12 | >12.5-20 | >20-25 | >25-35 | >35-50 | >50-100 | ||||
EH36 | Any | Plate/sheet | N,TM | ||||||
Profile steel | N(25),TM(25),AR*(15),CR*(15) | - |
A. Delivery Condition: As Rolled(AR), Controled Rolling(CR),Thermal Mechanical Control Process(TMCP),Normalizing(N),Tempering(T), Annealing(A), Quenching(Q), Quenching & Tempering(QT).
B. The Ultrasonic inspection can be done according to ASTM A435, ASTM A577, ASTM A578, EN10160, SEL072, NFA 04-305, BS5996 standard.
C. Additional Service: Heat treatment, Charpy V tes, Pre treatment,Cutting,Galvanization.
D. Classification Society like ABS , BV , DNV , GL, KR, LR, NK, RINA.
Contrast in the different standard
ASTM A131M | TOCT 5521 | BS LR | GB712 |
EH36 | E36 | EH36 | E36 |