Recommended method of application:
A. adjust carbon content while blending, add it into the place below the middle part of the electric furnace along with metal furnace charge when melting down liquid steel(iron) in accordance with the requirement of carbon content, absorptivity of carbon could reach 90%-95%, during strong carburant residue shall not appear, otherwise it is easy to be wrapped in the non-waste residue and influence the absorption of carbon thereby.
calcined petroleum coke is widely used for steel-smelting, casting, brake pedal and friction material.
NO. | Fixed Carbon | Sulphur | Moisture | Volatile | Graininess |
>= | <= | <= | <= | Granularity distribution 90% | |
T9830 | 98.50% | 0.30% | 0.50% | 0.50% | 1-5mm |
T9805 | 98.50% | 0.05% | 0.50% | 0.50% | 1-5mm |
T9850 | 98.50% | 0.50% | 0.50% | 0.80% | 1-5mm |
T9530 | 95.30% | 0.30% | 0.26% | 1.14% | 1-4mm |
T8520 | 85.00% | 0.20% | 0.30% | 1.20% | 1-5mm |
T8020 | 80.00% | 0.20% | 1.30% | 3.50% | 1-5mm |
grain size : 1-5mm,2-6mm,0-3mm or as per suctomer requirement.