Titanium mixed metal oxide coated tubular anode
Chemical Composition of substrate:
Titanium ASTM B338 Grade 1 or Grade 2
C | max 0.08% |
N | max 0.03% |
H | max 0.015% |
Fe | max 0.20% |
O | max 0.18% |
Residual | max each 0.1% |
Residual | max total 0.4% |
Ti | balance |
Coating Catalyst : mixed metal oxide
Specification:
Diameter (mm) | Wall Thickness (mm) | Length (mm) | Weight/PC (kg) | Surface Area/PC (m2) | Working life (year) |
16 | 1.0 | 1000 | 0.212 | 0.05 | >20 |
19 | 1.0 | 1000 | 0.254 | 0.06 | >20 |
25 | 1.0 | 1000 | 0.339 | 0.0785 | >20 |
25 | 1.5 | 1000 | 0.498 | 0.0785 | >20 |
32 | 1.0 | 1000 | 0.438 | 0.121 | >20 |
32 | 1.5 | 1000 | 0.646 | 0.121 | >20 |
The specification can be changed according to customer's request.
Tubular Anode Applications
The tubular anode can be made singly or in strings.
Suit for all natural environments, such as: soil, fresh water, sea water, mud.
The current output depends on the anode dimension, substrate, applications and design lifetime.
Advantages:
High current output and low electrical resistance.
Using tubular anodes can save 15-35% of install cost comparing to use other anodes.
Anode-cable assemblies are easy to hanlde,transport and install because of their unique flexbility.
Production Flow of MMO anode:
Raw material --- Shearing --- Machining ---welding--- Blasting --- Picking ----Automatic coating ---Inspection---Package
Production Equipment:
Testing Equipment:
Package of products: