Basic Info.
  • Brand Name: HN 
  • High compressive strength: 1h>25Mpa 
  • fast open traffic: 1hour 
  • High bending strength: 1h>5Mpa 
  • good adhesive performance: reach 2.8 Mpa 
  • good Impact resistant performance: 5-8 times than ordinary concrete 
  • No dry crack: after solidification. 
  • used for: high-speed,national,provincial,airports,and other transportaion 
  • package: 25kg 
  • Exporting countries: over 20 countries 
  • Model No.: QM 
  • Place of Origin: Henan  
  • Min.Order: 5 Ton
  • Means of Transport: Ocean, Air, Land
Supply Capacity
  • Production Capacity: 1000/month
  • Packing:25kg
  • Delivery Date: 5-7days

Over 10 years experience for  HuiNeng brand  bridge reinforcement repair product 

I. Introduction  of bridge reinforcement repair !

Deck concrete repair material (QM type) is a high-tech strength and good toughness
rapid repair material, ideal material suitable for highway, national, provincial,
municipal roads rapid repair of the bridge. The Department of Science and
Technology in Henan can bridge cement potholes Treatment, Treatment cement
pavement crack, crack Treatment bridge deck Treatment potholes, broken concrete
bridge expansion joints, potholes, cracks quickly repair areas with core technology!
Realized 1h fast open traffic!

2. product characteristics of bridge reinforcement repair  :

a: fast recovery of traffic: for high-speed, national, provincial, municipal, airports and
other transportation can be achieved 1 hours.
b: high compressive strength: 1h more than 25Mpa, 2h more than 35Mpa, 1d more
than 60Mpa, 28d more than 80Mpa.
c: high flexural strength: 1h greater than 5Mpa, 2h greater than 7.5Mpa, 1d more than
10Mpa, 28d more than 11Mpa.
d: good adhesion properties: bond pull strength reaches 2.8Mpa, to solve the
traditional material bond is not strong or problems can easily lead hollowing cracks.
e: the product toughness and impact resistance: 5-10 times that of ordinary concrete.
f: the thermal expansion coefficient: basically consistent with the primary concrete.
g no shrinkage cracks: between the original concrete and no shrinkage cracks after
solidification.
h: frost and salt corrosion: cold-resistant, corrosion-resistant sulfate, non-toxic,
non-corrosive.


3: Construction process and successful cases

 

4:certification of bridge reinforcement repair :

 5: the detected value:

Test items

Unit

Technical Requirements

Test results

Individual conclusions

Setting time

Initial setting

Min

≥20

25

Meet the requirements

Final setting


≤60

30

Compressive strength

2h

Mpa

≥20

33.0

Meet the requirements

1d


≥40

66.1

28d


≥50

90.5







Drawing strength

28d

Mpa

≥2.0

2.8

Meet the requirements

Expansion

28d

/

0.00%-0.1%

0.01%

Meet the requirements

 6:package of process:

7:our service:

 weclome to contact us we will reply you as soon as possible !



Send message to this supplier
Ms. alisa (saler)
Tel: 86-371-65775236
Mobile: 13526768303
Enter between 20 to 3,000 chatacters.
Contact Method
Henan Huineng Road And Bridge Technology Co.ltd.
Mazhai Industrial Estate, Erqi District, Zhengzhou, Henan, China (Mainland) / 450000
Didn't find what you're looking for? Post Buying Lead or contact our customer service specialist for help!
Buyer Help Center