titanium alloy plate TC17 titanium alloy bar raw materiasl in stock
It is beta phase titanium alloy solid solution consisting of a single phase alloy, is not heat treatment, it has high strength, get into the system of titanium alloy alloy after quenching and aging dagger step reinforcement, strength at room temperature can reach 1372-1666 MPa;But, the poor thermal stability should not be used at high temperature.
1. specification
ASTM B348 , ASTM F136/67,ASME SB348,AMS 4928, MIL
Rolled Bars Dia. (2.0-45) * ≥1000mm
Forged Bars Dia. (50-400) * ≤6000mm
Length: 50mm~6000mm, as requested
2. Features
Low density,High specific strength,Excellent corrosive resistance,Rustless,Good thermal stability, paper making, metallurgy, oil industry, Biological features,Plasticity,etc.
3. Applications
Chemical industry,Petroleum chemical industry, medical
Textile printing and dyeing,
Construction field, Decoration,Seawater desalination,
4. Chemical composition TC 17
TC17 titanium alloy
titanium alloy plate TC17 titanium alloy bar raw materiasl in stock
It is beta phase titanium alloy solid solution consisting of a single phase alloy, is not heat treatment, it has high strength, get into the system of titanium alloy alloy after quenching and aging dagger step reinforcement, strength at room temperature can reach 1372-1666 MPa;But, the poor thermal stability should not be used at high temperature.
TC17 titanium alloy chemical composition
Grade | Main components% % | impurity /%,Not more than | |||||||||
AL | Mo | Mn | Sn | Fe | C | N | H | O | other | ||
single | total | ||||||||||
TC17 | 4.4~5.5 | 3.5~4.5 | 1.5~2.5 | 1.5-2.5 | 0.15~0.3 | 0.05 | 0.05 | 0.05 | 0.10 | 0.10 | 0.30 |