TP316Ti Stainless Steel Heat Exchanger Tube SS Seamless Pipes UNS S31635 WNR 1.4571

 

316Ti (UNS S31635) is a titanium stabilised version of 316 molybdenum-bearing austenitic stainless steel. The 316 alloys are more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels such as 304. They also offer higher creep, stress-rupture and tensile strength at elevated temperature. High carbon Alloy 316 stainless steel can be susceptible to sensitisation, the formation of grain boundary chromium carbides at temperatures between approximately 900 and 1500°F (425 to 815°C) which can result in intergranular corrosion. Resistance to sensitisation is achieved in Alloy 316Ti with titanium additions to stabilise the structure against chromium carbide precipitation, which is the source of sensitisation. This stabilisation is achieved by an intermediate temperature heat treatment, during which the titanium reacts with carbon to form titanium carbides. This significantly reduces susceptibility to sensitisation in service by limiting the formation of chromium carbides. Thus, the alloy can be used for extended periods at elevated temperatures without compromising its corrosion resistance. 316Ti has equvilent corrosion resistance to sensitisation as the low carbon version 316L.

 

Testings (Destructive, Non Destructive):

 

Positive Material Identification - PMI Testing


Chemical Analysis - Spectro Analysis


Mechanical Testing Such as Tensile, Elongation, Reduction of Area


Micro Test


Macro Test


Hardness Test


Pitting Resistance Test


Intergranular Corrosion (IGC) Test


Flaring Test


Flattening Test


Hydrostatic Test


Hydrogen-Induced Cracking (HIC) Test, NACE TM0284


Sulfide Stress Corrosion Cracking (SSC), NACE TM 0177


Radiography Test


Dye Penetrant Test (DP Test)


Ultra Sonic Test (UT)


Eddy Current Testing


Impact Test


Bend Test

 

Mechanical Properties:

 

Temper Annealed
Tensile Rm 75 ksi (min)
Tensile Rm 515 MPa (min)
R.p. 0.2% Yield 30 ksi (min)
R.p. 0.2% Yield 205 MPa (min)
Elongation (2” or 4D gl) 35 % (min)


Physical Properties (Room Temperature):

Specific Heat (0-100°C) 500 J.kg-1.°K-1
Thermal Conductivity 14.6 W.m -1.°K-1
Thermal Expansion 16.5 mm/m/°C
Send message to this supplier
Mr. Mr. Will Ma
Tel: 86-21-57701837
Enter between 20 to 3,000 chatacters.
Contact Method
SpezillaTubeCompanyLimited
No.18 Baosheng Road, Songjiang District,undefined, Shanghai, China (Mainland)
Didn't find what you're looking for? Post Buying Lead or contact our customer service specialist for help!