HONGDA Manual electrostatuc spray paint gun
if Poor paint atomizing
1. too low in atomizing air pressure
2. too much injected paint
3. too high in viscosity of paint
4. bent the electrode pin of nozzle
5. damaged nozzle
6. not suitable solvent
7. not adequate clearance between air guide and jet
solution & improvements
boost air pressure up
adjust injection to low or boost atomizing air pressure
adjust the viscosity of paint to low
repair it or replace it with a new one
repair it or replace it with a new one
consult to HI MI sunac or paint manufacture
adjust clearance to be approx 2mm (one rete:1mm)
Max voltage DC-60KV hydraulic pressure Max 0-0.3Mpa standard 0.6Mpa air pressure Max 0.05-0.5Mpa standard 0.06Mpa air consumption 350Nl/mm ari bore screw bore PF 1/4 paint bore screw bore PF 1/4 Length 248mm supply cable (standard) 5M/6M/8M/10M weight(without nozzle & cables) 480g