Quick Details
Place of Origin: TIANJIN China (Mainland) | Brand Name: BAIGUAN | Model Number: ER5356 ER4043 |
Material: Aluminum / Aluminum Alloy | Diameter: 0.8-2.5 | Melting Point: 500 |
Weight: 1kg 2kg 5kg 15kg | Application: welding machinery | material: aluminum |
Surface Treatment: Color Coated | Application: dicine machinery manufacturing | Alloy Or Not: Non-alloy |
Wire Gauge: 0.8MM-2.0MM | Ultimate Strength (≥ MPa): 170-250mpa | Al (Min): 30% |
Conductivity: good | Elongation (≥ %): 100mm |
Packaging & Delivery
Packaging Detail: | mig automatic welding wire(plastic spool tight-packing 20kg/apool 15kg/spool 5kg/spool 1kg/spool) TIG Argon arc welding wire(packing in drums 1m/line,5kg/drum,10kg/drum) |
Delivery Detail | 15-20days |
Specifications
Aluminum alloy rod Specialized in production pure aluminum welding rod, aluminum magnesium welding rod, aluminum silicon wel
We are professional manufactory for the aluminum welding wire, load in Ningbo of China, E110 Aluminum welding wire/rod
Aluminum Welding wire Specialized in production pure aluminum welding rod, aluminum magnesium welding rod, aluminum silicon welding rod, low silicon welding rod, high silicon welding rod.The product surface is luminous, and the welding performance is good. It is used in each kind of aluminum material welding.
Technology data for your reference:
AWS | Joint Strength | Parent metal | Characteristics |
Standard | (Mpa) | ||
ER1070 | Above 55 | Pure aluminum series105010701080 | Good anti-corrosive and plasticity |
ER1100 | 80-110 | Pure aluminum series1100 | Good anti-corrosive and plasticity |
ER1200 | 80-110 | Pure aluminum series1200 | Good anti-corrosive and plasticity |
ER2319 | 400-450 | Pure aluminum series2219 | High intensity after heat treatment |
ER4043 | 170-250 | Al-Mg-Si casting aluminum | The anti-thermal crack performance of the welded joint is good, but the plasticity, toughness are low, becomes grey black after anodic process |
ER4047 | 170-250 | Casting Al. ,Al-Cu casting ,Ag-Mg-Si casting | The anti-thermal crack performance of the welded joint is good, but the plasticity, toughness are low, becomes grey black after anodic process |
ER4145 | 200-300 | Al-Cucasting20142017 | The anti-thermal crack performance of the welded joint is good, but the plasticity, toughness are low, becomes grey black after anodic process |
ER5554 | 180-240 | low Mg content5052,5454casting | Use chemical equipment with a temperature above 65 |
ER5654 | 210-270 | medium Mg content5154casting | medium intensity,good anti-corrosive |
ER5356 | 270-310 | Al-Mg casting, Al-Mg-Si casting, Al-Zn-Mg casting | Typical welding wire used most widely, good mechanics performance and anti-corrosiveness |
ER5556 | 280-320 | Al-Zn-Mg casting, Al-Mg casting | The connector intensity is high, and the moulding performance and tenacity is inferior to 5183 |
ER5183 | 280-310 | Al-Mgcasting5083 | Typical welding wire used most widely, good mechanical performance and anti-corrosiveness |