Sintered alnico magnet possesses high magnetic density and great time stability and low coefficient of temperature, so under the quick change of temperature the demagnetization is low. Because of high hardness, it's only fit for grind.
Sintered Alnico magnets are suitable for being used in instrument, meter, micro-motor, electro-acoustic device, microwave device and magnetic drive unit etc.
Sintered Alnico magnets are suitable for being used in instrument, meter, micro-motor, electro-acoustic device, microwave device and magnetic drive unit etc.
Grade | Br | bHc | iHc | (BH)max | Density | Tc | Remark | ||||
KGs | T | KOe | KA/m | KOe | KA/m | MGOe | KJ/m3 | g/cm3 | o C | Isotropic | |
FLN8 | 5.2 | 0.52 | 0.5 | 40 | 0.54 | 43 | 1.0-1.25 | 8-10 | 6.8 | 760 | |
FLNG12 | 7.0 | 0.7 | 0.5 | 40 | 0.54 | 43 | 1.5-1.75 | 12-14 | 7.0 | 810 | |
FLNGT14 | 5.7 | 0.57 | 0.95 | 76 | 0.98 | 78 | 1.75-2.0 | 14-16 | 7.1 | 850 | |
FLNGT18 | 5.6 | 0.56 | 1.1 | 88 | 1.13 | 90 | 2.25-2.75 | 18-22 | 7.2 | 850 | |
FLNG28 | 10.5 | 1.05 | 0.58 | 46 | 0.59 | 47 | 3.5-4.15 | 28-33 | 7.2 | 850 | Anisotropic |
FLNG34 | 11.0 | 1.1 | 0.63 | 50 | 0.64 | 51 | 4.3-4.8 | 34-38 | 7.2 | 890 | |
FLNGT28 | 10.0 | 1.0 | 0.7 | 56 | 0.71 | 57 | 3.5-3.8 | 28-30 | 7.2 | 850 | |
FLNGT31 | 7.8 | 0.78 | 1.3 | 104 | 1.13 | 90 | 3.9-4.5 | 31-36 | 7.2 | 850 | |
FLNG33J | 6.5 | 0.65 | 1.7 | 135 | 1.88 | 150 | 4.15-4.5 | 33-36 | 7.2 | 850 | |
FLNGT38 | 8.0 | 0.8 | 1.55 | 123 | 1.58 | 126 | 4.75-5.3 | 38-42 | 7.2 | 850 | |
FLNGT42 | 8.8 | 0.88 | 1.5 | 120 | 1.53 | 122 | 5.3-6.0 | 42-48 | 7.25 | 850 |