Core technology is the rise in recent years as a means of refining furnace is widely used in modern practice of steel wire feeding technology.Alloy cored wire can used to purity the liquid steel to practice,to change inclusion morphology properties of the alloy, can significantly improve the recovery rate,reduce training costs of steel,it's economic effect is remarkable.
Packing:
1.Vertical coils in steel cages on wooden (or steel) pallets, plastic shrink wrapped, labeled.
2. According to customers' requirement.
1.Vertical coils in steel cages on wooden (or steel) pallets, plastic shrink wrapped, labeled.
2. According to customers' requirement.
Available diameter: 9mm, 13mm and 16mm.
Description | Composition | Application |
pure ca wire | Ca>98 | Modification of inclusions by combing with oxide inclusions and making it liquid at steel making temperatures, thereby avoiding nozzle clogging in continuous casting. Improving isotropic properties of steel. For Deoxidation along with modification of inclusions. For low silicon grade steels. |
CaSi wire | 28–30% Ca, 58–62% Si | |
CaFe | 30% Ca, 70% Fe | |
CaAlFe | 30% Ca, 25%Al Bal–Fe, | |
Calcium Aluminum Alloy | Ca–Al 75% [(Ca–75%–Al–25%) or (Ca–60%–Al–40%)]; Fe–25% | |
Al Cored Wire (Al) | 98% Al | For effective Deoxidation with higher efficiency than solid wire. Wire diameters upto 25 mm for large vessels |
Iron (Fe) | 99% Min. | For better control of superheat in tundish during continuous casting |