Magnetic properties of SmCo5 | |||||||||||||
Material | Grade | Remanence | Coercive Force | Intrinsic Coercive Force | Max. | Curie | Max. | Temperature | Temperature | ||||
energy product | Temperature | Operating | Coefficient | Coefficient | |||||||||
Temperature | of Br | of Hc | |||||||||||
Br | Hcb | Hcj | (BH)max | Tc | Tw | ||||||||
SmCo 5 | T | KGs | KA/m | KOe | KA/m | KOe | KJ/m 3 | MGoe | ° C | ° C | %° C | %° C | |
(Smpr)co 5 | YX- | 0.81-0.85 | 8.1- | 620-660 | 7.8- | 1194-1830 | 15-23 | 110-127 | 14-16 | 750 | 250 | -0.05 | -0.3 |
16 | 8.5 | 8.3 | |||||||||||
YX- | 0.85-0.9 | 8.5- | 660-700 | 8.3- | 1194-1830 | 15-23 | 127-143 | 16-18 | 750 | 250 | -0.05 | -0.3 | |
18 | 9 | 8.8 | |||||||||||
YX- | 0.9-0.94 | 9.0- | 680-725 | 8.5-9.1 | 1194-1830 | 15-23 | 150-167 | 19-21 | 750 | 250 | -0.05 | -0.3 | |
20 | 9.4 | ||||||||||||
YX- | 0.92-0.96 | 9.2- | 710-750 | 8.9-9.4 | 1194-1830 | 15-23 | 160-175 | 20-22 | 750 | 250 | -0.05 | -0.3 | |
22 | 9.6 | ||||||||||||
YX- | 0.96-1.0 | 9.6- | 730-770 | 9.2-9.7 | 1194-1830 | 15-23 | 175-190 | 22-24 | 750 | 250 | -0.05 | -0.3 | |
24 | 10 | ||||||||||||
SmCo 5 | YX- | 0.9-0.94 | 9.0- | 680-725 | 8.5-9.1 | 1433-1830 | 18-23 | 143-160 | 18-20 | 750 | 250 | -0.05 | -0.3 |
20s | 9.4 | ||||||||||||
YX- | 0.92-0.96 | 9.2- | 710-750 | 8.9-9.4 | 1433-1830 | 18-23 | 160-175 | 20-22 | 750 | 250 | -0.05 | -0.3 | |
22s | 9.6 | ||||||||||||
Low | LTc | 0.59-0.63 | 5.9- | 460-493 | 5.8-6.2 | 1430-1830 | 18-23 | 68-80 | 8.5-10 | 700 | 250 | Temperature | Temperature |
temperature coefficient | (YX- | 6.3 | Coefficient | ||||||||||
SmCo5 (SmGd)Co 5 | 10) | of Br %° C | |||||||||||
20-100° C | -0.004 | ||||||||||||
100-200° C | -0.021 | ||||||||||||
200-300° C | -0.042 | ||||||||||||
ce(coFecu) 5 | YX- | 0.70-0.74 | 7.0- | 358-390 | 4.5-4.9 | 358-478 | 4.5-6 | 80-103 | 10.0-13 | 450 | 200 | ||
12 | 7.4 | ||||||||||||
Magnetic properties of Sm2Co17 | |||||||||||||
Material | Grade | Remanence | Coercive Force | Intrinsic Coercive Force | Max. | Curie | Max. | Temperature | Temperature | ||||
energy product | Temperature | Operating | Coefficient | Coefficient | |||||||||
Temperature | of Br | of Hc | |||||||||||
Br | Hcb | Hcj | (BH)max | Tc | Tw | ||||||||
Sm2Co17 | YXG- | 0.95-1.02 | 9.5- | 700-750 | 8.7-9.4 | 1990 | 25 | 175-191 | 22-24 | 800 | 350 | -0.03 | -0.2 |
Sm 2 | 24H | 10.2 | |||||||||||
(CoFecuzr)17 | YXG- | 1.02-1.05 | 10.2- | 750-780 | 9.4-9.8 | 1990 | 25 | 191-207 | 24-26 | 800 | 350 | -0.03 | -0.2 |
26H | 10.5 | ||||||||||||
YXG- | 1.03-1.08 | 10.3- | 756-796 | 9.5-10 | 1990 | 25 | 207-220 | 26-28 | 800 | 350 | -0.03 | -0.2 | |
28H | 10.8 | ||||||||||||
YXG- | 1.08-1.10 | 10.8- | 788-835 | 9.9-10.5 | 1990 | 25 | 220-240 | 28-30 | 800 | 350 | -0.03 | -0.2 | |
30H | 11 | ||||||||||||
YXG- | 0.95-1.02 | 9.5- | 700-750 | 8.7-9.4 | 1433 | 18 | 175-191 | 22-24 | 800 | 300 | -0.03 | -0.2 | |
24 | 10.2 | ||||||||||||
YXG- | 1.02-1.05 | 10.2- | 750-780 | 9.4-9.8 | 1433 | 18 | 191-207 | 24-26 | 800 | 300 | -0.03 | -0.2 | |
26 | 10.5 | ||||||||||||
YXG- | 1.03-1.08 | 10.3- | 756-796 | 9.5-10 | 1433 | 18 | 207-220 | 26-28 | 800 | 300 | -0.03 | -0.2 | |
28 | 10.8 | ||||||||||||
YXG- | 1.08-1.10 | 10.8- | 788-835 | 9.9-10.5 | 1433 | 18 | 220-240 | 28-30 | 800 | 300 | -0.03 | -0.2 | |
30 | 11 | ||||||||||||
YXG- | 1.02-1.05 | 10.2- | 750-780 | 9.4-9.8 | 955-1273 | 12.0-16 | 191-207 | 24-26 | 800 | 300 | -0.03 | -0.2 | |
26M | 10.5 | ||||||||||||
YXG- | 1.03-1.08 | 10.3- | 756-796 | 9.5-10.0 | 955-1273 | 12.0-16 | 207-220 | 26-28 | 800 | 300 | -0.03 | -0.2 | |
28M | 10.8 | ||||||||||||
YXG- | 1.08-1.10 | 10.8- | 788-835 | 9.9-10.5 | 955-1273 | 12.0-16 | 220-240 | 28-30 | 800 | 300 | -0.03 | -0.2 | |
30M | 11 | ||||||||||||
YXG- | 1.02-1.08 | 10.2- | 398-445 | 5.0-5.6 | 400-520 | 5.2-6.5 | 207-220 | 26-28 | 800 | 250 | -0.03 | -0.2 | |
28L | 10.8 | ||||||||||||
YXG- | 1.08-1.15 | 10.8- | 398-445 | 5.0-5.6 | 400-520 | 5.2-6.5 | 220-240 | 28-30 | 800 | 250 | -0.03 | -0.2 | |
30L | 11.5 | ||||||||||||
Low | LTC | 0.94-0.98 | 9.4- | 668-715 | 8.4-9.0 | 1194-1591 | 15-20 | 167-183 | 21-23 | 840 | 300 | Temperature | Temperature |
temperature coefficient Sm2Co17 (SmEr) 2 | (YXG- | 9.8 | Coefficient | ||||||||||
(CoTM) 17 | 22) | of Br %° C | |||||||||||
-50-25° C | 0.005 | ||||||||||||
20-100° C | 0.012 | ||||||||||||
100-200° C | 0.006 | ||||||||||||
200-300° C | -0.025 | ||||||||||||
Characteristic comparisons of permanent magnetic materials: | |||||||||||||
Materials | (BH)max | Hcj | Br Tc | (Working temperature)max | Anti-causticity | ||||||||
SmCo1: 5 | 16-25 | 15-25 | -0.05 | 200-250 | Good | ||||||||
SmCo2: 17 | 22-30 | 6.0-30 | -0.03 | 300-350 | Good | ||||||||
NdFeB | 26-52 | 12.0-30 | -0.11 | 80-200 | Bad | ||||||||
Ferrite magnet | 3-4.5 | 3-4.5 | -0.19 | 200-300 | Good | ||||||||
AINiCo | 5.0-10 | 1-1.8 | -0.03 | 450-500 | Excellent |