Specifications of Carpenter Alloy Rod
Rod Size | diameter: 3mm above, length: 20mm above |
Chemical composition of Carpenter Alloy Rod
Carbon | 0.02% |
Silicon | 0.35% |
Iron | Bal. |
Manganese | 0.50% |
Nickel | 48.00% |
Physical properties of Carpenter Alloy Rod
Specific Gravity | 8.18 |
Density | 0.2950 lb/n3 |
Mean specific heat | 0.1200 Btu/lb/oF |
Thermal conductivity | 90.20 Btu-in/he/ft2/oF |
Curie Temperature | 840 – 930 oF |
Melting Point | 2600oF |
Properties of Carpenter Alloy Rod
- Resistance to atmosphere corrosion factors
- Resistance to moisture corrosion
Applications of Carpenter Alloy Rod
1. Laminated cores in transformers and magnetic shields
2. Solenoid cores