2. Applied fields
1. Iron mines
2. Rare earth
3. Metal mines
4. Cement plant
5. Power station
6. All kinds of mines
7. Quartz sand mine
8. Chemical industry
9. Molybdenum mineral
10. Building material
11. Refractory industry
3.Chemical elements
Name | C | Si | Mn | Cr | Mo | V | Ti | Ni | Cu | P | S |
High Manganese Steel Liner | 1.1-1.4 | 0.3-1.0 | 11-14 | 0-2.5 | 0-0.5 | 0-0.5 | 0-0.2 | <0.5 | 0.2-1.0 | - | - |
middle alloy plate | 0.38-0.45 | 1-1.6 | 1.5-2.8 | 1.5-3 | 0.1-0.4 | 0-0.5 | 0-0.2 | <0.5 | 0.2-1.0 | - | - |
Multi element alloy plate | 1.5-2.5 | 0.5-0.8 | 0.6-1.0 | 3-5 | 0.15-0.3 | 0-0.5 | 0-0.2 | <0.5 | 0.5-1.0 | - | - |
High Manganese Steel hammerhead | 1.17-1.25 | ≤0.5 | 18.0-19.0 | ≤1.8 | - | - | - | - | 0.5-1.0 | ≤0.05 | ≤0.01 |
Mechanical Data
Name | Hardness (HRC) | Impelling strength (J/cm2) | Grinding loss (g/Ton) | Broken (%) | Working life (month) |
High Manganese Steel Liner | HB≤240 | 80-140 | ----- | ------- | Cement≥12 |
middle alloy plate | 48-55 | 20-25 | ----- | ------- | Cement≥30 |
Multi element alloy plate | 50-58 | 15-20 | ------ | ------- | Cement≥16 |
High Manganese Steel hammerhead | 60-65 | 6-10 | ------ | 0 | Higher than High Manganese Steel 1 times |