0.08mm PVC coated overlay with High-co 2750 oe or low-co 300oe magnetic strip for card making
Specifications:
Material | PVC material |
Thickness |
1.0mm ,0.08mm, 0.06mm thickness |
Type | High-co/Low-co magnetic strips |
Layout |
5*5 , 3*8 sheets |
Strips | Max. 8 strips |
Steps to make cards:
- Put printing core and two overlays together, then put into the laminator.(the laminating temperature and time is determined as per the instruction of the machine).Please be noticed that all glue sides of both PVC sheets and overlays are put inward.
- Lamination lasts 10-15 minutes. The pressure is 6-8Mpa.The temperature is 120-140°C.
- Cutting the card.
Technical note:
In manufacturing process, it can be directly laminated with PVC printing sheet, simplify the fabrication process, save time, adhesive strength is high.