PET drawbench production line:
First is the extruder temperature control is in commonly 250 ℃ ~ 280 ℃. Next up is cooling, take out after high temp
PP pack to bring the fracture parameters and elongation: tension
First is the extruder temperature control is in commonly 250 ℃ ~ 280 ℃. Next up is cooling, take out after high temp
PP pack to bring the fracture parameters and elongation: tension
1, 12 mm wide and 0.6 mm thick specifications of pure PP packing material with the fracture tension > 1000 N elongation: < 20%
2 and 13.5 mm wide and 0.6 mm to 0.8 mm thick specifications of pure PP packing material with the fracture tension: 1000 N-1500 N elongation: < 20%
3 and 15.5 mm wide and 0.6 mm to 0.8 mm thick rules and pure PP packing material with the fracture tension: 1500 N-2000 N elongation: < 20%
4, 19 mm wide 0.6 mm to 0.8 mm thick rules and pure PP packing material with the fracture tension: 2000 N