202 NO.1 stainless steel pipe
There is also should be minimized p, Sb, Bi, As impurities, such as content. Additionally optional A-F dual phase steel, which is not sensitive to stress corrosion in Cl- and OH- media. When fine cracks of the initial encounter ferrite does not continue to expand, ferrite content should be at around 6.
There is also should be minimized p, Sb, Bi, As impurities, such as content. Additionally optional A-F dual phase steel, which is not sensitive to stress corrosion in Cl- and OH- media. When fine cracks of the initial encounter ferrite does not continue to expand, ferrite content should be at around 6.