TSY-20 Geosynthetics material creep test system, used for determination of geotextile
and its related products tensile creep and tensile creep rupture performance test. Conform
to the standard ISO 13431, GB/T 17637, 50 t1129 JTG E, SL/T235-1999.
Technical parameters:
★Capacity:180KN Accuracy:≦±1%
★Width of the jig:50mm or 200mm Can be choose
★Creep space effectively:900mm,Effective width of test:350mm
★Accuracy of displacement measurement:0.03mm
★Time measurement error:≦±1%
contact us with skype=chinesemoulds (at)hotmail.com
and MSN is same skype.