Roadphalt colored epoxy asphalt pavement

Price: 2800.0 USD
Trade Term: FOB,CFR,CIF,DAT,FAS,DDP,DAP,CIP,CPT,FCA,EXW
Payment Terms: T/T,L/C,D/A,D/P,WU,Money Gram
Trade on HiSupplier, Worry Free Guarantee
Trading safety, secure your money, lower the risk, protect both buyers and suppliers
HiSupplier is a Chinese multinational company in U.S, it helps to coordination and order landing.
More ›
  • Product Details
  • Company Profile
  • Product Reviews
Basic Info.
  • Brand Name: RPT 
  • Place of Origin: Shanghai  
  • Min.Order: 1 Ton
  • Means of Transport: Ocean, Air, Land
Supply Capacity
  • Production Capacity: 500 Ton/Tons per Day
  • Packing:200 kg/ barrel
  • Delivery Date: 15-30days after payment by sea

Roadphalt colored modified asphalt 

l Product profile

Roadphalt colored asphalt is a new environment protection product which is developed independently by Shanghai Roadphalt Asphalt Technology Co. Ltd. Through 3 years' research, and has achieved a national patent and two national utility patents. It is Shanghai high-technology achievement transformation project and Shanghai innovation fund project, and it also passes SGS environmental monitoring. As high-performance asphalt modifier, polymer, coloring agent, anti-aging agent, high-viscosity asphalt stabilizer, anti-rutting agent and other additives are added, the product has some good performances such as economy, environmental protection, high temperature stability, good resistance to water damage, good construction performance and meeting the requirement of characteristic of heavy traffic asphalt. Now, our company offers a warming filling delivery (20-30 tons/jar, can dock batching plant), on-site processing (Mobile processing equipment of colored modified asphalt, 25 tons/batch, can dock batching plant) and drum transport (200Kg / barrel, need take off the barrel of equipment).

 

Moveable storage tank of colored modified asphalt for batching plant can dock pipeline of batching plant, and no new equipments are added and just clean the original pipeline of black asphalt, no dumping equipments and no storage tanks of colored modified asphalt are needed, and the loss is almost zero. Furthermore, the remaining colored asphalt and pigment can be returned if packaging is not damaged. 

 

After our technicians enter the field and complete the docking of batching plant and processing equipment, products can be supplied, and the daily amount of feeding is 5,000-20,000m2 for paving (determined by production of batching plant and paving rate). Time is unlimited and operation is easy. When mixture is prepared, 2-3% pigment is put into batching plant and mixed with stone to form colored asphalt mixture, then loading and paving can be done. 3 cm of paving thickness is suggested on the premise of saving cost. The product has also advantages of high strength for colored pavement, high and low-temperature performance, excellent durability. In addition, color is bright and colorfast. Pigment package is 25 kg / bag.

 

Roadphalt Pigment of colored asphalt

No.

Type

Composition

Cost

Range of selective color

Recommendation degree

1

red

ferric oxide

lower

Subject to actual example

★★★★★

2

green

chrome oxide

higher

Subject to actual example

★★★★

3

yellow

chrome oxide

higher

Subject to actual example

★★★☆

4

blue

cobalt oxide

higher

Subject to actual example

★★

5

brown

composite ferric oxide

lower

Subject to actual example

★★★★☆

6

dark brown

composite pigment

normal

Subject to actual example

★★★★☆

7

white

zirconia oxide

highest

Subject to actual example

★★★

Note: If colored stone is added, color can be maintained for many years (adjust the amount of additives according to customers).    

 

Modified decolored asphalt ( RPT-A )

Property index

 

Unit

Requirement

Penetration(25℃)

 

0.1mm

50-70

Softening point 

 

〉48

Ductility(15℃)

 

cm

〉60

TFOT Thin-film Oven Test ( 163℃, 5h )

 

 

Mass loss

%

〈 3

 

Penetration ratio of bitumen

%

〉50

in barrel

in bulk

putting into mixing position from the viewing port 

docking asphalt pipeline

viewing port

Our company can send engineers to assist successful completion of the construction project, and the quality of project is ensured.

 On-site feeding 

 

The docking of mobile equipment and batching plant

 scope:

1. Road pavement (service life is over 5 years)

Cycle path

Sidewalk

Parking

Landscape garden

 

Construction guide  

 

Mixing and transport of mixture

 

Construction technology of colored asphalt mixture is similar to that of common asphalt mixture, and attention should be paid to the following: 


1. Clean the original feed pipeline of black asphalt and dock the equipment of colored asphalt. 

 

2. Before mixing, mixing tank in the mixing station is washed with hot aggregate several times cleanly.

 

3. Property of raw material should be stable so that mix proportion of production target can be close to that of design target greatly. 

4. Temperature of aggregate is controlled at 170degree-190degree, and heating temperature of asphalt is at 160degree-175degree. 

5. Pigment is packed in bag. Pre-calculate the amount of pigment for a jar of mixture before using and open package in advance. After aggregate is put into mixing tank, pigment is added directly. The suggested mixing time is 60s, and actual mixing time depends on the requirements of appearance for asphalt. Asphalt mixture should have performances of even coverage, no gray particle, uniform color, no agglomerate and no isolation phenomena of particle. The quality can meet construction requirement.

6. Vehicles and coverings for transporting mixture should be cleaned in advance. 

Mixture paving 

1. The paving processes of both colored asphalt mixture and conventional asphalt mixture are basically the same. 

2. Paver should be cleaned, especially screed should be cleaned with solvent or colored asphalt mixing is paved on the pavement substrate until there are no streaks from the substrate to the superstratum. 

3. When paving begins, production, transport, paving and rolling performance of mixture should be considered to ensure continuous paving and full-size shape for keeping color consistent, granule uniform and beautiful. 

 

Compaction molding of mixture

1. Water in the roller tank should be replaced, and rust should be cleaned. Roller should be stopped on the mat so that it does not touch the substrate of black asphalt, and rolls on directly from wooden pad to colored mixture. Any tools touched with mixture in the rolling process should be cleaned.

2. Rolling compaction combination: the same with conventional permeable asphalt mixture

3. Rolling strength: compaction should be guaranteed on the premise of no crushed stone. Over compaction should be avoided, or colored effect is affected if stone is crushed.

4. When the rolling starts, because there is some water on the surface, manual operation, manual paving and manual feeding must be stopped, or it is difficult for substrate mixture and artificial feeding to bond together. This should be emphasized by construction staff in advance. 

 

Note: traffic is opened after rolling is over and temperature is cooled to room temperature.

 

 

 

 

Working drawing of colored asphalt pavement

Feeding              Paving              Rolling             Molding   

 

Preparation conditions of mixture and construction temperature

 

Mixing

Construction

Temperature of stone

Temperature of asphalt

Mixing temperature

Initial rolling

Final rolling

170℃-190℃

160℃-175℃

160℃-175℃

Above 120℃

Above 100℃

 



Send message to this supplier
Ms. Gina
Tel: 86-21-55781851-8025
Enter between 20 to 3,000 chatacters.
Contact Method
Shanghai Roadphalt Asphalt Technology Co.,Ltd
Room709-711,NO.3,Oriental Blue Ocean International Plaza,No.1800 Huangxing Road, Yangpu District,200433., Shanghai, China (Mainland)
Didn't find what you're looking for? Post Buying Lead or contact our customer service specialist for help!
Buyer Help Center