SmCo magnets is also named with SmCo magnetic steels, SmCo permanent magnets, SmCo permanent magnetic iron and rare earth cobalt permanent magnet. It is one type rare earth material permanent magnet, and It is a high performance, low temperature coefficient permanent magnet with its high working temperature-350 degree centigrade. When working above 180 degree centigrade, its maximum energy prodcut BH and steady temperature are superior than NdFeB magnetic material. It needn't to be coated because it is difficult to be eroded and oxidized.
SmCo ring magnets widely used in transduces, instruments, etc.
The demagnetized curve of sintered Sm2Co17 magnet
Magnetic Characteristics of Sintered SmCo:
Materia | Grade | Max Engery product | Remanence | Coercive Force | Intrinsic Coercive Force | Temp Coeff | Density | Curie Temp | Working Temp |
(BH)max | Br | Hcb | Hcj | αBr | D | Tc | Tw | ||
KJ/m3(MGOe) | mT(KGs) | KA/m(KOe) | KA/m(KOe) | %/ ℃ | g/cm3 | ℃ | ℃ | ||
Sm1Co5 | 18A | 143(18) | 850(8.5) | 597(7.5) | 1273(16.0) | -0.04 | 8.2 | 740 | 250 |
18B | 143(18) | 850(8.5) | 660(8.3) | 1600(20.0) | |||||
19 | 150(19) | 900(9.0) | 690(8.7) | 900(11.3) | |||||
20A | 159(20) | 900(9.0) | 613(7.7) | 1989(25.0) | |||||
20B | 160(20) | 900(9.0) | 660(8.3) | 900(11.3) | |||||
20C | 160(20) | 900(9.0) | 680(8.5) | 1270(16.0) | |||||
21 | 165(21) | 920(9.2) | 710(8.9) | 1600(20.0) | |||||
22A | 175(22) | 940(9.4) | 700(8.8) | 900(11.3) | |||||
22B | 180(22) | 950(9.5) | 720(9.0) | 1270(16.0) | |||||
Sm2Co17 | 24C | 191(24) | 1000(10.0) | 356(4.5) | 413(5.2) | -0.03 | 8.3 | 820 | 350 |
24D | 190(24) | 1000(10.0) | 480(6.0) | 560(7.0) | |||||
24E | 190(24) | 1010(10.1) | 675(8.5) | 1300(16.0) | |||||
24F | 190(24) | 980(9.8) | 710(8.9) | 900(11.3) | |||||
24G | 190(24) | 1000(10.0) | 740(9.3) | 2070(26.0) | |||||
24H | 195(24) | 1020(10.2) | 748(9.4) | 1433(18.0) | |||||
25 | 205(26) | 1040(10.4) | 700(8.8) | 1300(16.0) | |||||
26A | 205(26) | 1020(10.2) | 420(5.2) | 440(5.5) | |||||
26B | 207(26) | 1030(10.3) | 716(9.0) | 1432(18.0) | |||||
26C | 210(26) | 1020(10.2) | 740(9.3) | 900(11.3) | |||||
26D | 205(26) | 1050(10.5) | 756(9.5) | 1433(18.0) | |||||
26E | 210(26) | 1070(10.7) | 780(9.8) | 2070(26.0) | |||||
28A | 220(28) | 1080(10.8) | 420(5.2) | 440(5.5) | |||||
28B | 223(28) | 1100(11.0) | 438(5.5) | 454(5.7) | |||||
28C | 220(28) | 1090(10.9) | 520(6.5) | 560(7.0) | |||||
28D | 224(28) | 1110(11.1) | 640(8.0) | 1040(13.0) | |||||
28E | 225(28) | 1060(10.6) | 760(9.6) | 900(11.3) | |||||
28F | 220(28) | 1080(10.8) | 780(9.8) | 955(18.0) | |||||
28G | 220(28) | 1100(11.0) | 820(10.3) | 2070(26.0) | |||||
30A | 240(30) | 1100(11.0) | 780(9.8) | 900(11.3) |
The demagnetized curve of sintered Sm2Co17 magnet