Gray cast iron material.
Working surface finished by hand scraping, it is widly used to test the straightness and flatness of workpiece and equipment installing. Best working temperature 20±5°C.
Working surface finished by hand scraping, it is widly used to test the straightness and flatness of workpiece and equipment installing. Best working temperature 20±5°C.
Specification (mm) | Straightness and Flatness of Working Surface | Parallelism Between Working Surfaces | ||||
Accuracy Grade (μm) | ||||||
0 | 1 | 2 | 0 | 1 | 2 | |
500×35 | 3 | 6 | 12 | 4.5 | 9 | 18 |
750×40 | 4 | 8 | 15 | 6 | 12 | 25 |
1000×50 | 5 | 10 | 20 | 7.5 | 15 | 30 |
1250×50 | 12 | 24 | 18 | 36 | ||
1600×70 | 15 | 30 | 20 | 40 | ||
2000×80 | 18 | 36 | 27 | 54 | ||
2500×80 | 44 | 65 | ||||
3000×100 | 52 | 78 | ||||
3500×100 | 60 | 90 | ||||
4000×100 | 68 | 100 |
Specification (mm) | Straightness and Flatness of Working Surface | Parallelism Between Working Surfaces | ||||
Accuracy Grade (μm) | ||||||
0 | 1 | 2 | 0 | 1 | 2 | |
500×35 | 3 | 6 | 12 | 4.5 | 9 | 18 |
750×40 | 4 | 8 | 15 | 6 | 12 | 25 |
1000×50 | 5 | 10 | 20 | 7.5 | 15 | 30 |
1250×50 | 12 | 24 | 18 | 36 | ||
1600×70 | 15 | 30 | 20 | 40 | ||
2000×80 | 18 | 36 | 27 | 54 | ||
2500×80 | 44 | 65 | ||||
3000×100 | 52 | 78 | ||||
3500×100 | 60 | 90 | ||||
4000×100 | 68 | 100 |