SteelMaterial | 38CrMoALA,SKD61,SKD11,D2etc. |
Hardnessafter Hardening & Tempering | HB240-280 |
NitridingTreatment Time | ≥ 96hours |
NitridedLayer Hardness | 950-1020Hv |
NitridedLayer Thickness | 0.5-0.8mm |
SurfaceRoughness | Ra0.4um |
SurfaceHardness | 58-64HRC |
ScrewStraightness | 0.015mm |
Chromium-PlatedSurface Hardness After Nitriding | ≥ 900HB |
Chromium-PlatingLayer Thickness | 0.05-0.10mm |
BimetallicLayer Hardness | 50-65HRC |
DepthOf Alloy Layer | 0.8-2.0mm |