Specification
Rod Size | diameter:3mm above, length: 20mm above |
Chemical composition
Ni | 65% |
Mo | 28.5% |
Cr | 1.5% |
Fe | 1.5% |
Co | 3% |
W | 3% |
Mn | 3% |
Physical Properties of Hastelloy B-3 Rod
Density | 9.22 g/cm3 | 0.333 lb/in3 |
Melting Point | 1418oC | 2585oF |
Coefficient of expansion | 10.6µm/m°C (20 - 100°C) | 5.7x10-6 in/in°F (70 - 212°F) |
Modulus of Rigidity | 83 kN/mm2 | 12038 ksi |
Modulus of Elasticity | 216 kN/mm2 | 31329 ksi |
Mechanical properties of Hastelloy B-3 Rod
Condition | Tensile Strength | Service temperature | ||
Annealed | 1000-1200 N/mm2 | 145 - 174 ksi | -200 to +400oC | -330 to +750oF |
SpringTemper | 1600-2000 N/mm2 | 232 - 290 ksi | -200 to +400oC | -330 to +750oF |
Characteristics of Hastelloy B-3 Rod
- Hefty resistance to strongacids
- Resistance to pittingcorrosion and stress corrosion cracking
- Highly ductile
Applications of Hastelloy B-3 Rod
1.Chemical processes
2. Vacuum Furnaces
3. Mechanical components in reducing environments.